U.M. | ||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Compression strength | > 97 | N/mm2 | ||||||||||||
Bending strength | > 30 | N/mm2 | ||||||||||||
Elastic modulus | 9290 | N/mm2 | ||||||||||||
Adhesion to dry concrete | > 4 | N/mm2 | ||||||||||||
Adhesion to damp concrete | > 2 | N/mm2 | ||||||||||||
Adhesion to steel | > 3,5 | N/mm2 | ||||||||||||
Glass transition point (calorimetric method) | ca. 53 | °C | ||||||||||||
Density | 1,95 | kg/dm3 | ||||||||||||
A + B mixture ratio | 100 + 6 |
Temperature | Use (pot-life) | hardening | ||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
10 °C | 80' | 10 hours | ||||||||||||
20 °C | 60' | 6 hours | ||||||||||||
30 °C | 45' | 4 hours |